Preparation and Characterization of Coaxial Electrospinning rhBMP2-Loaded Nanofiber Membranes

Table 1

The ingredients of each sample for test.

SampleInner layerOuter layerAbbreviations

1PLLA/HFIP 6 wt.%Zein/HFIP (14 wt.%)Zein/PLLA
2PLLA/HFIP 6 wt.%Zein/HFIP (14 wt.%)+DEXZein-DEX/PLLA
3PLLA/HFIP 6 wt.% + 12 μg rhBMP2Zein/HFIP (14 wt.%)Zein/PLLA-rhBMP2 (12 μg)
4PLLA/HFIP 6 wt.% + 30 μg rhBMP2Zein/HFIP (14 wt.%)Zein/PLLA-rhBMP2 (30 μg)
5PLLA/HFIP 6 wt.% + 48 μg rhBMP2Zein/HFIP (14 wt.%)Zein/PLLA-rhBMP2 (48 μg)
6PLLA/HFIP 6 wt.% + 12 μg rhBMP2Zein/HFIP (14 wt.%)+DEXZein-DEX/PLLA-rhBMP2 (12 μg)
7PLLA/HFIP 6 wt.%+30 μg rhBMP2Zein/HFIP (14 wt.%)+DEXZein-DEX/PLLA-rhBMP2 (30 μg)
8PLLA/HFIP 6 wt.%+48 μg rhBMP2Zein/HFIP (14 wt.%)+DEXZein-DEX/PLLA-rhBMP2 (48 μg)