Research Article
Enhanced Photocatalytic Activity of TiO2/SnO2 Binary Nanocomposites
| Sample | Phase | (nm) | (nm) | (nm) | Crystallite size (nm) | Mass content (%) |
| P25TiO2 | Anatase | 0.378 | 0.378 | 0.950 | 4.4 | 75 | Rutile | 0.459 | 0.459 | 0.296 | 4.0 | 25 | sTiO2 | Anatase | 0.378 | 0.378 | 0.947 | 7.0 | 100 | Р25TiO2-SnO2 | Anatase | 0.379 | 0.379 | 0.950 | 15.2 | 69 | Rutile | 0.459 | 0.459 | 0.296 | 20.1 | 21 | SnO2 | 0.475 | 0.475 | 0.319 | 11.6 | 10 | s1TiO2-SnO2 | Anatase | 0.379 | 0.379 | 0.945 | 5.7 | 89 | SnO2 | 0.497 | 0.497 | 0.497 | 5.2 | 11 | s2TiO2-SnO2 | Anatase | 0.379 | 0.379 | 0.949 | 7.0 | 89 | SnO2 | 0.483 | 0.483 | 0.321 | 6.8 | 11 |
|
|