Research Article

Optimization on Powder Metallurgy Process Parameters on Nano Boron Carbide and Micron Titanium Carbide Particles Reinforced AA 4015 Composites by Taguchi Technique

Table 1

Process parameters for compacting Al+micron TiC+nano B4C powder.

Parameter for the processRangeUnits

Sintering time2, 2.25, 2.5hr
Sintering temperature620, 640, 660°C
Compacting pressure300, 350,400MPa