Optimization on Powder Metallurgy Process Parameters on Nano Boron Carbide and Micron Titanium Carbide Particles Reinforced AA 4015 Composites by Taguchi Technique

Table 7

Compression strength and sound to noise ratio value of Al AA4015+TiC+B4C sorted materials.

Exp no.123456789

Sintering time (hr)2222.252.252.252.52.52.5
Sintering temp (°C)620640660620640660620640660
Compaction pressure (MPa)300350400350400300400300350
Compression pressure (MPa)329.36300.06314.16300.11291.47296.19297.26292.55301.5
S/N ratio (dB)52.51851.66752.08751.66851.40151.54851.58151.43551.711