S. noNormalizedGRCsGRGRank
Wear indexLoss of volumeWear indexLoss of volume

10.968421.01340.94561.0000.98342
20.97420.99760.94610.98420.96641
30.79140.80160.70520.72310.716116
4000.33410.33420.343312
50.95410.97450.91250.94680.92873
60.95850.98120.91820.95430.93514
70.12830.09610.37430.36610.371214
80.63420.64190.28120.57580.584215
91.01240.90411.01460.83490.91145
100.79650.80740.71420.71240.71246
110.93470.95460.88320.91280.897211
120.78300.78160.69500.70420.691010
130.81240.81680.73460.74560.939813
140.86140.83420.77890.79540.77859
150.84310.86430.76320.78690.77697
160.90120.92430.84340.86610.85348