Research Article

Conductometry and Size Characterization of Polypyrrole Nanoparticles Produced by Ball Milling

Figure 1

SEM images of PPy particles taken after (a) 60 min, (b) 120 min, (c) 180 min, (d) 240 min, and (e) 300 min.
690407.fig.001a
(a)
690407.fig.001b
(b)
690407.fig.001c
(c)
690407.fig.001d
(d)
690407.fig.001e
(e)