Research Article

Comparative Assessment of Antimicrobial Efficiency of Ionic Silver, Silver Monoxide, and Metallic Silver Incorporated onto an Aluminum Oxide Nanopowder Carrier

Figure 3

XRD diffractograms obtained for the Al2O3-Ag+ nanopowder (a), intermediary product after the thermal decomposition conducted at a temperature of 700°C for 24 h (Al2O3-Ag2O) (b), and the final product after the reduction process conducted at a temperature of 700°C for 2 h in H2 (Al2O3-Ag) (c). The final product contained 2.84 wt% of silver.
263583.fig.003a
(a)
263583.fig.003b
(b)
263583.fig.003c
(c)