Microporosity Development of Herringbone Carbon Nanofibers by RbOH Chemical Activation
Figure 3
Proportion of ultramicropores (0.7 nm), supermicropores (0.7–2 nm), and mesopores (2–50 nm) at different (a) RbOH/CNFs ratio, (b) activation temperatures, and (c) He flow rates. (Activation conditions are showen in Table 1.)