Research Article

A Preliminary Investigation of Ductility-Enhancement Mechanism through In Situ Nanofibrillation in Thermoplastic Matrix Composites

Figure 7

Nonreversible heat flow MDSC thermogram of unprocessed as-received HMD Xenoy composite pellet compared with those of undeformed tensile specimen and the fractured region of a room temperature quasistatic tensile-tested tensile specimen; both tensile specimens were injection molded at a nominal shear rate of 28ā€‰sāˆ’1.
424015.fig.007