Thermal properties of the unfilled and talc filled TPU/PP blends.
| Sample | (°C) | (°C) | Δ (J/g) | Δ (J/g) | (%) |
| TPU/PP 80/20 | 163.4 | 111.4 | 15.0 | 9.3 | 9.1 | TPU/T/PP 80/5/20 | 163.0 | 118.1 | 24.0 | 28.0 | 14.5 | TPU/PP 50/50 | 164.3 | 110.0 | 42.1 | 45.8 | 25.5 | TPU/T/PP 50/5/50 | 163.0 | 117.5 | 46.6 | 53.8 | 28.2 | TPU/PP 20/80 | 164.3 | 111.3 | 74.1 | 77.4 | 45.0 | TPU/T/PP 20/5/80 | 164.0 | 120.0 | 77.9 | 79.8 | 47.2 |
|
|