Table of Contents
Journal of Powder Technology
Volume 2013, Article ID 946984, 5 pages
http://dx.doi.org/10.1155/2013/946984
Research Article

Improvement of the Contact Strength of Al2O3/SiC by a Combination of Shot Peening and Crack-Healing

Faculty of Engineering, Yokohama National University, 79-5 Tokiwadai, Hodogaya-ku, Yokohama 240-8501, Japan

Received 1 March 2013; Accepted 25 April 2013

Academic Editor: Kotoji Ando

Copyright © 2013 Tomoya Oki et al. This is an open access article distributed under the Creative Commons Attribution License, which permits unrestricted use, distribution, and reproduction in any medium, provided the original work is properly cited.

Linked References

  1. W. Pfeiffer and T. Frey, “Strengthening of ceramics by shot peening,” Journal of the European Ceramic Society, vol. 26, no. 13, pp. 2639–2645, 2006. View at Publisher · View at Google Scholar · View at Scopus
  2. K. Tanaka, Y. Akiniwa, and Y. Morishita, “Residual stress distribution in the sub-surface region of shot-peened ceramics,” Nihon Kikai Gakkai Ronbunshu, A Hen/Transactions of the Japan Society of Mechanical Engineers, Part A, vol. 71, no. 12, pp. 1714–1721, 2005. View at Google Scholar · View at Scopus
  3. W. J. Moon, T. Ito, S. Uchimura, and H. Saka, “Toughening of ceramics by dislocation sub-boundaries,” Materials Science and Engineering A, vol. 387–389, no. 1-2, pp. 837–839, 2004. View at Publisher · View at Google Scholar · View at Scopus
  4. S. R. Choi and V. Tikare, “Crack healing behavior of hot pressed silicon nitride due to oxidation,” Scripta Metallurgica et Materiala, vol. 26, no. 8, pp. 1263–1268, 1992. View at Google Scholar · View at Scopus
  5. M. C. Chu, S. Sato, Y. Kobayashi, and K. Ando, “Damage healing and strengthening behaviour in intelligent mullite/SiC ceramics,” Fatigue and Fracture of Engineering Materials and Structures, vol. 18, no. 9, pp. 1019–1029, 1995. View at Google Scholar · View at Scopus
  6. K. Ando, B. S. Kim, M. C. Chu, S. Saito, and K. Takahashi, “Crack-healing and mechanical behaviour of Al2O3/SiC composites at elevated temperature,” Fatigue and Fracture of Engineering Materials and Structures, vol. 27, no. 7, pp. 533–541, 2004. View at Publisher · View at Google Scholar · View at Scopus
  7. K. Takahashi, M. Yokouchi, S. K. Lee, and K. Ando, “Crack-healing behavior of Al2O3 toughened by SiC whiskers,” Journal of the American Ceramic Society, vol. 86, no. 12, pp. 2143–2147, 2003. View at Google Scholar · View at Scopus
  8. K. Takahashi, Y. Nishio, Y. Kimura, and K. Ando, “Improvement of strength and reliability of ceramics by shot peening and crack healing,” Journal of the European Ceramic Society, vol. 30, no. 15, pp. 3047–3052, 2010. View at Publisher · View at Google Scholar · View at Scopus
  9. K. Takahashi and Y. Nishio, “Improvement of the contact strength of Si3N4/SiC by a combination of shot peening and crack-healing,” Journal of Solid Mechanics and Materials Engineering, vol. 3, no. 1, pp. 41–52, 2012. View at Google Scholar
  10. T. Oki, Master Thesis in Yokohama National University, 2013.
  11. R1607, Testing Method for Fracture Toughness of Fine Ceramics, Japan Standards Association, 1995.