Response, response time, and recovery time of Pd modified Pd-Ag/ZnO Schottky sensor with different concentrations of CH4 in nitrogen and in synthetic air as the carrier gas (calculated from Figure 9).

% of CH4ResponseResponse time (s)Recovery time (s)
N2 as carrier gasSynthetic air as carrier gasN2 as carrier gasSynthetic air as carrier gasN2 as carrier gasSynthetic air as carrier gas


0.0118.26.810.213.818.720.0
0.0522.311.06.79.917.219.7
0.123.217.06.038.716.817.7
0.525.217.84.027.216.117.0
132.224.82.694.616.015.9