Research Article

Organic Membranes for Selectivity Enhancement of Metal Oxide Gas Sensors

Figure 9

Separation properties of PET and PEN upon exposure to 150 ppm H2, 30 ppm CO, 1,000 ppm CH4, 500 ppm ethanol, 500 ppm acetone, and 25 ppm acetaldehyde. The diameter of the membranes is 6.4 mm.
(a)
(b)