Research Article
A Study on Coloring Properties of Rheum emodi on Jute Union Fabrics
Table 2
Printed sample coding.
| Fabric | Sample code | Mordant + thickener | Sample code | Mordant + thickener |
| Untreated jute/cotton
| UJC1 | No mordant + guar gum | UJC1′ | No mordant + albumin | UJC2 | Alum + guar gum | UJC2′ | Alum + albumin | UJC3 |
CuSO4 + guar gum | UJC3′ | CuSO4 + albumin | UJC4 | FeSO4 + guar gum | UJC4′ | FeSO4 + albumin |
| Myrobalan treated jute/cotton | MJC1 | Alum + guar gum | MJC1′ | Alum + albumin | MJC2 | CuSO4 + guar gum | MJC2′ | CuSO4 + albumin | MJC3 | FeSO4 + guar gum | MJC3′ | FeSO4 + albumin |
| Untreated jute/wool
| UJW1 | No mordant + guar gum | UJW1′ | No mordant + albumin | UJW2 | Alum + guar gum | UJW2′ | Alum + albumin | UJW3 | CuSO4 + guar gum | UJW3′ | CuSO4 + albumin | UJW4 | FeSO4 + guar gum | UJW4′ | FeSO4 + albumin |
| Myrobalan treated jute/wool
| MJW1 | Alum + guar gum | MJW1′ | Alum + albumin | MJW2 | CuSO4 + guar gum | MJW2′ | CuSO4 + albumin | MJW3 | FeSO4 + guar gum | MJW3′ | FeSO4 + albumin |
|
|