Research Article
Durability Environmental Regionalization for Concrete Structures
Table 4
Result of durability environmental regionalization for concrete structures in Shenzhen city.
| Regions | Weight of durability environmental regionalization indexes | Geographical area | Surface chloride concentration | Concrete carbonation depth | Ambient temperature | Ambient relative humidity |
| I | 0.3154~0.4250 | 0.1803~0.2560 | 0.0154~0.1737 | 0.0213~0.3125 | A narrow distribution along the coastline, mainly in the south of Guangzhou-Shenzhen highway |
| II | 0.2758~0.3239 | 0.2445~0.3460 | 0.0758~0.1239 | 0.0250~0.2375 | Central of Bao’an district, northern of nanshan and Futian District, most parts of the Luohu and Yantian district, southern of Longgang district |
| III | 0.1762~0.2618 | 0.3219~0.4795 | 0.0758~0.1998 | 0.0219~0.1843 | Mainly in the north of Longda expressway, huiyan Highway, and Shenzhen-Shantou expressway |
|
|