Research Article

Parameter Optimization of Polishing M300 Mold Steel with an Elastic Abrasive

Figure 9

Surface topographies of the workpiece by optimized parameters before and after polishing (S=1200#, Wt=4500r/min, Ap=0.25mm, and Vf=0.8mm/min).
(a) Initial surface morphology
(b) Surface morphology polished