Research Article
Nonlinear Analysis for the Crack Control of SMA Smart Concrete Beam Based on a Bidirectional B-Spline QR Method
Table 5
The recovery situation of maximum crack width with different thickness of concrete cover.
| Temperature of SMA wires (°C) | Maximum crack width (mm) | Recovery rate of maximum crack width (%) | | | | | | |
| 20 | 0.2098 | 0.2848 | 0.3700 | 0.00 | 0.00 | 0.00 | 40 | 0.2090 | 0.2838 | 0.3687 | 0.39 | 0.37 | 0.34 | 60 | 0.1940 | 0.2625 | 0.3403 | 7.54 | 7.82 | 8.04 | 80 | 0.1851 | 0.2501 | 0.3234 | 11.77 | 12.19 | 12.58 | 100 | 0.1795 | 0.2422 | 0.3129 | 14.44 | 14.97 | 15.43 | 120 | 0.1779 | 0.2399 | 0.3098 | 15.22 | 15.78 | 16.26 |
|
|
Concrete covers : mm, mm, and mm.
|