Experimental orthogonal array design and corresponding results.

PQCVMaterial removal rate (mm3/min)Surface roughness (μm)

33332.62962.394
33312.653352.413
33112.512751.52
31133.36491.8145
33132.736951.501
22232.702752.28
22222.71132.318
13313.069452.584
11313.45232.6125
32222.645752.1185
23222.5082.204
21222.622952.299
22222.59162.318
12222.82912.3275
22222.77972.413
31312.81962.508
22222.780652.337
22323.07612.546
11333.19962.5935
11113.253751.881
22222.731252.318
22222.61822.3275
22123.118851.672
31132.476651.596
22212.702752.318
13313.46941.786
13333.56631.7575
31312.402551.653
31332.81962.489
13332.86332.5745