Scanning / 2017 / Article / Fig 5

Research Article

Wear Characteristic of Stellite 6 Alloy Hardfacing Layer by Plasma Arc Surfacing Processes

Figure 5

Wear rate of Stellite 6 under different loadings at room temperature and 300°C.