Research Article
Structural and Kinetic Hydrogen Sorption Properties of Zr0.8Ti0.2Co Alloy Prepared by Ball Milling
Table 2
EDS results of elemental composition for selected regions of
samples after ball milling for different time.
| ZrCo samples | Selected region | Zr (atomic%) | Ti (atomic%) | Co (atomic%) | Fe (atomic%) | (Zr + Ti)/(Co + Fe) |
| BM 0 h | 1# | 38.26 | 9.73 | 52.01 | | | 2# | 38.49 | 7.48 | 54.04 | | | Average | 38.38 | 8.61 | 53.03 | | 0.89 |
| BM 2 h | 1# | 36.47 | 8.40 | 44.56 | 10.58 | | 2# | 34.26 | 7.77 | 46.27 | 11.71 | | Average | 35.37 | 8.09 | 45.42 | 11.15 | 0.77 |
| BM 4 h | 1# | 35.34 | 9.26 | 44.3 | 11.11 | | 2# | 32.49 | 8.06 | 47.85 | 11.60 | | Average | 33.92 | 8.66 | 46.08 | 11.36 | 0.74 |
| BM 6 h | 1# | 37.43 | 8.71 | 45.97 | 7.90 | | 2# | 28.83 | 7.2 | 56.89 | 7.08 | | Average | 33.13 | 7.96 | 51.43 | 7.49 | 0.70 |
| BM 8 h | 1# | 32.78 | 8.37 | 49.28 | 9.58 | | 2# | 29.61 | 8.52 | 52.36 | 9.51 | | Average | 31.20 | 8.45 | 50.82 | 9.55 | 0.66 |
|
|