Sets of parameters used in the study.
| No. | Energy input (J/mm3) | Cathode current (mA) | Scanning speed (mm/s) |
| 1 | 10 | 4.5 | 5400 | 2 | 9.5 | 11,400 | 3 | 14.5 | 17,400 | 4 | 19.5 | 23,400 |
| 5 | 20 | 4.5 | 2700 | 6 | 9.5 | 5700 | 7 | 14.5 | 8700 | 8 | 19.5 | 11,700 |
| 9 | 30 | 4.5 | 1800 | 10 | 9.5 | 3800 | 11 | 14.5 | 5800 | 12 | 19.5 | 7800 |
| 13 | 40 | 4.5 | 1350 | 14 | 9.5 | 2850 | 15 | 14.5 | 4350 | 16 | 19.5 | 5850 |
| 17 | 50 | 4.5 | 1080 | 18 | 9.5 | 2280 | 19 | 14.5 | 3480 | 20 | 19.5 | 4680 |
|
|