Research Article
In Vivo Corrosion Behavior of Biodegradable Magnesium Alloy by MAF Treatment
Figure 7
Observations of in vivo experimental samples before and after corrosion using FE-SEM. Surface morphology of (a) Bare, 0 week; (b) Bare, 16 weeks; (c) MAF, 0 week; and (d) MAF, 16 weeks.
(a) |
(b) |
(c) |
(d) |