Stress Corrosion Cracking Behavior of TP 439 and 690 TT under Film-Forming Amine Environment

Figure 7

The fracture morphologies for TP 439 SS after SSRT in argon atmosphere.
(a) Overview
(b) Central area
(c) Marginal zone
(d) Marginal zone