Review Article
Processing of Aluminium-Silicon Alloy with Metal Carbide as Reinforcement through Powder-Based Additive Manufacturing: A Critical Study
Table 5
Effect of MC on mechanical properties of Al-Si alloy.
| MCs with % of weight/volume | Matrix | Wear resistance | Coe. of friction | Tensile property | % elongation | Process |
| TiC—30% Vol. | AlSi12 | ++ | | | | DED | TiC—3% Wt. | AlSi10Mg | + | - | + | + | SLM | TiC—5% Wt. | AlSi10Mg | + | - | ++ | + | SLM | TiC—5% Wt. | AlSi10Mg | + | - | + | + | DED | TiC—5% Wt. | AlSi15 | + | - | + | + | SLM | TiC—10% Wt. | AlSi15 | + | - | -- | - | SLM | TiC—1 : 1 | Al9.8Si0.6MgTi | | | + | + | SLM | TiC—5% Wt. | AlSi10Mg | | | ++ | ++ | SLM | SiC—15% Wt. | AlSi10Mg | + | | - | - | SLM | SiC—5% Vol. | AlSi10Mg | | | | | SLM | SiC—10% Vol. | AlSi10Mg | | | | | SLM | SiC—15% Wt. | Al | + | - | | | SLM | SiC—5 to 15% Vol | Al–7Si–0.3Mg | | | | | Laser sintering | SiC—20% Wt. | AlSi10Mg | ++ | -- | | | SLM | SiC—12% Vol. | Al-12Si | | | | | SLM | B4C—20% Wt. | AlSi10Mg | + | - | | | SLM |
|
|
+, increase; ++, drastic increase; -, decrease; --, drastic decrease; , no observation. |