Research Article
Study on the Comprehensive Properties and Microstructures of A3-3 Matrix Graphite Related to the High Temperature Purification Treatment
Table 4
Oxidation corrosion rate and ash content of MG pebbles lathed before and after HTP.
| Samples | MG pebbles 1 | MG pebbles 2 | MG pebbles 3 | Specification | Average | Deviation | Average | Deviation | Average | Deviation |
| Oxidation corrosion rate (mg·cm−2 h−1) | 0.48 | 0.03 | 0.50 | 0.04 | 1.55 | 0.01 | ⩽1.3 | Ash content (ppm) | 15.15 | 0.35 | 15.80 | 0.46 | 31.7 | 2.12 | ⩽300 |
|
|