Research Article
Experimental Research on Dynamic Behavior of Circular Mild Steel Plates with Surface Cracks Subjected to Repeated Impacts in Low Temperature
Figure 14
Maximum lateral plastic deformation at different temperatures. (a) L/D = 1/3. (b) L/D = 1. (c) L/D = 5/3.