Research Article
Metalized Plastic Waste Fiber Effects on Green Concrete Beams Mechanical Performance
Table 2
Composition of cementitious materials and aggregates.
| Compound (%) | Cement | Silica fume | Zeolite | Gravel | Sand |
| CaO | 64.14 | 0.59 | 5.48 | 42.50 | 17.20 | SiO2 | 22.92 | 92.64 | 68.69 | 8.90 | 50.40 | Al2O3 | 4.13 | 0.53 | 14.96 | 0.80 | 6.30 | Fe2O3 | 2.81 | 1.05 | 3.95 | 1.60 | 6.90 | L.O.I | 2.43 | 0.47 | 1.05 | 39.80 | 9.20 | MgO | 1.92 | 1.60 | 1.30 | 5.60 | 6.50 | K2O | 0.85 | 1.64 | 2.12 | 0.20 | 0.80 | Na2O | 0.44 | 0.82 | 1.85 | 0.20 | 2.10 | Other | 0.36 | 0.66 | 0.60 | 0.40 | 0.6 |
|
|