Macroporosity of fresh and used active cokes.

Active cokeAC0AC33ACS0ACS33

Macroporescm3/gcm3/gcm3/gcm3/g
5–100 nm0.0230.0140.1010.017
100–1000 nm0.0930.0760.1180.042
1000–7500 nm0.0550.0310.0220.124

Total macropores0.1710.1210.2410.183