Research Article

Direct Synthesis and Morphological Characterization of Gold-Dendrimer Nanocomposites Prepared Using PAMAM Succinamic Acid Dendrimers: Preliminary Study of the Calcification Potential

Figure 6

Gold-dendrimers Au-G6-2.5 formation and evolution over 24 hours as recorded by UV-VIS measurements; absorbance was recorded at moment 0, 23 minutes, 25 minutes, 60 minutes, 120 minutes, 205 minutes, 235 minutes, 252 minutes, 300 minutes, 400 minutes, and 24 hours after synthesis, respectively.
103462.fig.006