Research Article

Effect of Repeated Thermal Shock on Mechanical Properties of ZrB2-SiC-BN Ceramic Composites

Figure 6

Surface micrographs of ZSB materials after thermal shock for 30 times: (a) 1200°C; (b) 1400°C; (c) 1600°C; (d) 1800°C.
419386.fig.006a
(a)
419386.fig.006b
(b)
419386.fig.006c
(c)
419386.fig.006d
(d)