Research Article

Evaluation of Varying Ductile Fracture Criteria for 42CrMo Steel by Compressions at Different Temperatures and Strain Rates

Figure 4

The damage distribution of the height reduction of 60% at temperature 1348 K and strain rate 0.01 s−1.