Research Article

A Novel Study of Methane-Rich Gas Reforming to Syngas and Its Kinetics over Semicoke Catalyst

Table 3

Surface area, pore volume, and pore size of semicoke.

Sample Surface area/m2 g−1Pore volume/cm3 g−1Pore size/nm

Before reaction15.1920.0098.735
After reaction18.4180.0137.116