Research Article

The Effect of Prophylactic Polishing Pastes on Surface Roughness of Indirect Restorative Materials

Figure 4

(a) Scanning electron micrograph of GE2-C group showed a homogeneous surface. (b) GE2-DT showed some slight scratch lines while (c) GE2-TP revealed some defects and scratches.
962764.fig.004a
(a)
962764.fig.004b
(b)
962764.fig.004c
(c)