Research Article
The Process of Nanostructuring of Metal (Iron) Matrix in Composite Materials for Directional Control of the Mechanical Properties
Figure 8
XRD spectrum of samples of dispersed iron with titanium-carbon nanostructures after treatment with 10 cycles of ALD reactions and sintered at 1100°C.