Research Article
Variation of Bulk Modulus, Its First Pressure Derivative, and Thermal Expansion Coefficient with Applied High Hydrostatic Pressure
Table 2
Values of thermal expansion coefficient.
| Element | αv × 10−6 per k | Reference |
| Potassium | 249 | [77] | Aluminum | 75 | [78] | Beryllium | 34.8 | [79] | Gold | 41.7 | [77] | Copper | 49.8 | [78] | Tantalum | 19.8 | [77] | Cobalt | 37.2 | [77] | Molybdenum | 15.6 | [77] | Tungsten | 13.8 | [77] |
|
|