Research Article
Improved Indium-Free Transparent ZnO/Metal/ZnO Electrode through a Statistical Experimental Design Method
Figure 4
(a) Depth profile of Cu ion in the ZCZ multilayer as-prepared and after annealing at 300°C for 20 min and (b) dependence of resistance of ZCZ on the postannealing temperature.
(a) |