Analysis of the Processes in Spent Fuel Pools in Case of Loss of Heat Removal due to Water Leakage

Figure 7

Heat generated by oxidation: (a) heat generation due to fuel cladding oxidation in air and steam during whole period of accident, (b) slow heat generation due to fuel cladding oxidation at temperature below 1200°C heat generation due to intensive fuel cladding oxidation in steam at temperature higher than 1200°C.