Review Article
Biomass to Bioethanol: Initiatives of the Future for Lignin
Table 1
Tensile strength test using LPF resin as an adhesive.
| Samples | Maximum load (N) | Ultimate tensile strength (MPa) | Elongation at break (%) |
| 1 | 3823.50 | 15.39 | 1.84 | 2 | 2944.85 | 11.78 | 1.32 | 3 | 1866.08 | 7.51 | 0.33 |
| Mean | 2878.14 | 11.56 | 1.163 |
|
|