Results of wood particleboard bonded with glyoxalated organosolv lignin-mimosa tannin formulation [
58].
| | | | | IB | Formulation | Press time (mn) | Temperature | Density (kg/m3) | N/mm² = Mpa |
| Lignin (50%) + tannin (50%) | 7.5 min | 195°C | 695 | | Lignin (40%) + tannin (60%) | 7.5 min | 195°C | 696 | |
|
|