Research Article

Tribological Behavior of Hastelloy C and Refractalloy 26

Figure 2

Microstructure of the Hastelloy C prior to testing (a) and that of the alloy subjected to the thermal cycle of the wear test at 400°C (b), as well microstructure of the Refractalloy 26 without modifications (c) and once it had been subjected to the thermal cycle of the same test (d).
650562.fig.002a
(a)
650562.fig.002b
(b)
650562.fig.002c
(c)
650562.fig.002d
(d)