Research Article
Surface Characteristics and High Cycle Fatigue Performance of Shot Peened Magnesium Alloy ZK60
Figure 2
Section topographies of the peened ZK60-T5 alloy at different Almen intensities: (a) 0.05 mmN; (b) 0.10 mmN; (c) 0.30 mmN; (d) 0.40 mmN.