Utilization of Agroresidual Waste in Effective Blending in Portland Cement
Table 2
Composition of OPC used in this study.
| ||||||||||||||||||||||||
The mix design used for casting was 1 : 1.5 : 3. Water-to-cement ratio was (w/c) = 0.53. |
| ||||||||||||||||||||||||
The mix design used for casting was 1 : 1.5 : 3. Water-to-cement ratio was (w/c) = 0.53. |