Effects of Different Artificial Agings on Structure and Properties of Whatman Paper Samples
Figure 3
WAXS intensity profiles of Whatman paper: (A) unaged; (B) undergone to thermal degradation; (C) undergone to accelerating aging in climatic chamber; (D) undergone to chemical degradation; (E) undergone to photo-oxidation.