Research Article
Properties of High-Strength Flowable Mortar Reinforced with Palm Fibers
Table 3
Mortar mixes proportions.
| Index | Cement Kg/m3 | Silica fume Kg/m3 | Water Kg/m3 | Sp. Kg/m3 | Sand Kg/m3 | W/B | palm fiber volumetric fraction % | Flow mm |
| M0 | 550 | 40 | 240 | 11.8 | 1415 | 0.43 | 0 | 140 | M1 | 550 | 40 | 240 | 11.8 | 1415 | 0.43 | 0.2 | 130 | M2 | 550 | 40 | 240 | 11.8 | 1415 | 0.43 | 0.4 | 125 | M3 | 545 | 40 | 240 | 11.8 | 1405 | 0.43 | 0.6 | 125 | M4 | 545 | 40 | 240 | 11.8 | 1405 | 0.43 | 0.8 | 120 | M5 | 540 | 40 | 240 | 11.8 | 1390 | 0.43 | 1.0 | 115 | M6 | 540 | 40 | 240 | 11.8 | 1390 | 0.43 | 1.2 | 120 | M7 | 535 | 40 | 240 | 11.8 | 1380 | 0.43 | 1.4 | 115 | M8 | 535 | 40 | 240 | 11.8 | 1380 | 0.43 | 1.6 | 110 |
|
|