Thermal Expansion Behaviour of Ternary Nickel-Based, Cobalt-Based, and Iron-Based Alloys Containing Very High Fractions of Carbides
Table 3
Thermal expansion coefficients measured on the dilatometry curves, deformation at reaching 1200°C, deformation and total deformation values after the 1200°C-isothermal stage () and after return to 100°C ()—iron-based alloys.
Temperature (°C)
Average linear thermal expansion coefficient (×10−6°C−1)