Surface Modification of Light Alloys by Low-Energy High-Current Pulsed Electron Beam

Figure 6

Evolution of cross-section microhardness with depth for the LEHCPEB-treated samples: (a) AZ31 Mg alloy (27 kV, 10 pulses); (b) AZ91 Mg alloy (27 kV, 10 pulses); (c) pure Mg (27 kV, 10 pulses); (d) pure Al (28 kV, 1 pulse).