Electrosynthesis and Spectroscopic Characterization of Poly(o-Aminophenol) Film Electrodes
Figure 17
(a) In-situ UV-Vis spectra of POAP at different applied electrode potentials. The POAP film was prepared on ITO coated glass at 0.8 V (1 h electrolysis) from a solution containing 0.05 M o-AP in 0.5 M H2SO4 solution. (b) Enlarged spectra of (a) between 320 and 450 nm [19].