Research Article
Infiltration Kinetics of Wetting in a Building Plaster and the Effect of Added Glass and Hemp Fibers
Table 8
Capillary absorption capacity and sorptivity.
| | Plaster | PGF | PHF |
| (kg·m−2·s−0.5) | 0.416 | 0.363 | 0.156 | (cm·s−1/2) by (21) | 0.099 | 0.087 | 0.041 | (cm·s−1/2) by gravimetry [9] | 0.095 | 0.096 | 0.078 |
|
|