Research Article

Evaluation Effects of the Short- and Long-Term Freeze-Thaw Exposure on the Axial Behavior of Concrete-Filled Glass Fiber-Reinforced-Polymer Tubes

Figure 5

Signs of degradation of PCC at 300 F/T cycles before testing.
340672.fig.005