Research Article

Direct Fabrication of Cobalt Oxide Nanoparticles Employing Sucrose as a Combustion Fuel

Figure 3

XRD patterns of nanocrystalline Co3O4 samples calcined at 400°C being prepared at different F/O molar ratios: (a) 0.5, (b) 1, (c) 2, (d) 5, (e) 8, and (f) 16.